2 article(s) from Chang, Man-Ping
Figure 1: The physical model of the nano-punching system. (a) The punch is made of nickel, and the workpiece ...
Figure 2: The shear stress–displacement curves of O1, O2, and O3 orientations during the nano-punching proces...
Figure 3: The schematic diagram of the nano-punching process. (a) The elastic deformation stage, (b) the plas...
Figure 4: The atomic displacement vectors of O1, O2, and O3 during the punching process.
Figure 5: The shear stress distribution diagram of orientation O1, O2, and O3 during the punching process. Th...
Figure 6: The shear stress and strain distribution during the unloading process of the O1, O2, and O3 orienta...
Figure 7: The shear stress–displacement curves of workpieces with various thicknesses during the nano-punchin...
Figure 8: The fracture strength of the 5, 10, 15, and 20 Å workpieces.
Figure 9: The shear stress distribution diagram of the 5, 10, 15, and 20 Å workpieces during the punching pro...
Figure 10: The fracture strength of various workpiece clearances.
Figure 11: The shear stress distribution diagram of the 15 Å workpiece with 5, 10, 15, and 20 Å clearance valu...
Figure 12: The shear stress distribution diagram of the 20 Å workpiece with 5, 10, 15, and 20 Å clearance valu...
Figure 13: The fracture strength of the punch with various angles.
Figure 14: The shear stress distribution of θ = 5°, 10°, 15°, and 20° taper angles during the nano-punching pr...
Figure 1: Schematic of GPCuNL composite.
Figure 2: Two different graphene chiralities and the bond length of graphene.
Figure 3: Stress–strain curves of (a) zigzag and (b) armchair GPCuNL composites at different temperatures.
Figure 4: The shear modulus of GPCuNL composites at different temperatures and with different graphene chiral...
Figure 5: (a, c) Cross-sectional view of the CSP analysis of the GPCuNL composites and (b, d) DXA analysis of...
Figure 6: (a–f) Von Mises stress of graphene under shear loading along the zigzag direction at 300 K. (a–c) T...
Figure 7: (a, c) Cross-sectional view of the CSP analysis of the GPCuNL composites and (b, d) DXA analysis of...
Figure 8: (a–f) Von Mises stress of graphene under shear loading along the armchair direction at 300 K. (a)–(...
Figure 9: Out-of-plane displacement of graphene at different temperatures. (a1–a5) Zigzag graphene, (b1–b5) a...
Figure 10: Stress–strain curves of zigzag graphene/Cu composites with different repeat layer spacings.
Figure 11: The shear modulus of zigzag GPCuNL composites with different repeat layer spacings.
Figure 12: The out-of-plane displacement of zigzag graphene with different repeat layer spacings.
Figure 13: The DXA analysis of GPCuNL composites with different repeat layer spacings at 300 K. The magnified ...
Figure 14: Stress–strain curves of zigzag GPCuNL composites with different grain sizes.
Figure 15: Shear modulus of zigzag GPCuNL composites with different grain sizes.
Figure 16: The structural evolution of polycrystalline Cu with different grain sizes. The “PD” symbols represe...
Figure 17: The out-of-plane displacement of zigzag graphene in GPCuNL composites with different grain sizes.