Beilstein J. Nanotechnol.2013,4, 325–329, doi:10.3762/bjnano.4.37
. The average sample weights of approximately 15.0–17.5 mg were placed in the aluminium crucible. Heating rates of 20 °C min−1 were used in the temperature range 20–400 °C. The crystallinity (Tc) and melting temperature (Tm) were recorded as the inflection point of the increment of specificheat and as
PDF
Figure 1:
Stress–strain curves of Mater-Bi and Mater-Bi/FBC bionanocomposites: (a) pure Mater-Bi, (b) Mater-B...